Wap Edition | +86 731 84770165
Multilayer Bearing
Wrapped Bronze Bearing
Bimetal Bearing
Cast Bronze Bearing
Oil Sintered Bearing
Ball Cage Retainer
Ball Transfer Units
Adapter Sleeve
Lock Nut
Lock Washer
Withdrawal Sleeve
Lock card
COM folder cloth phenolic series
Fill modified fluorine plastic series
Hydraulic seal series
Spherical Plain Bearing
Maintenance-free Plain Bearing
Hot Products product is same as per standard ISO354(DIN1494)
  • Bronze bearing
  • GEH..XF Series Radial Spherical Plain Bearings
  • GEG..ETL GEG..XTL Series Radial Spherical Plain Bearings
  • GE..ETL GE..XTL Series Radial Spherical Plain Beariangs
  • GE..C GEG..C Series Radial Spherical Plain Bearings
  • GE..E, GE..ES, GE..ES-2RS Series Radial Spherical Plain Bearings

The most common failure of sliding bearing

2018-04-27

Hunan Jintai Hardware and Machinery Co., ltd. introduced sliding bearing at work because of journal and bearing shell exposure will clash, causing wear appearance fever, even "killed", so when planning bearing, should choose sliding bearing material manufacture with good sex of anti-friction bearings, choose suitable lubricant and adopt appropriate measures for the supply of improving the structure of the bearing for thick film lubrication, etc.

sliding bearing

1, tile surface corrosion: spectrum analysis found that abnormal non-ferrous metal element concentration;Iron spectrum presented many nonferrous metal composition of sub-micron wear particles;Lubricating oil water overruns, acid value, overspending.
2, shaft neck appearance corrosion: spectrum analysis found that abnormal iron concentration, there are a lot of iron in iron spectrum of submicron particles, oil water overruns or acid value overruns.
3, a shaft neck appearance strain: iron spectrum have iron series cutting grinding grain or black oxide particles, metal appearance exists heat tint.
4, tile back micro wear: abnormal spectral analysis found that iron concentration, there are a lot of iron in iron spectrum wear submicron particles, abnormal oil moisture and acid value.
5, a bearing surface strain: iron spectrum found cutting abrasive, abrasive ingredients for non-ferrous metal.
6, tile surface peeling: finds many large-scale iron spectrum fatigue peeling alloy wear particles, the layered grits.
7, bearing tile burning: iron spectrum have more large-scale alloy grinding grain and black metal oxides.


Hunan Jintai Hardware and Machinery Co.,Ltd. is a professional manufacturer on various kind of bearings over 15 years China factory.
We are making all kinds of slide bearings including 
DU PTFE composit bushing, DX POM composite bushing,bimetal bushing,wrapped bronze bushing, cast sliding bushings and wear plate bearing pad, sintered bronze bushing and sintering parts, ball transfer bearings, etc.
The shapes of bearings can be in sleeve, flanged, spherical, plate, washer, pad, ring, square etc.
Base materials in carbon steel, harden steel, iron, stainless steel, bronze, brass, copper, bronze-steel alloy.Lubricant materials in PTFE, teflon, POM, nylon, plastic, oil, graphite, grease, MoS2, etc.
Export to America,Canada,Brazil,Peru,Argentina,Chile,Paraguay,Europe,Finland,France,Germany,Italy,Spain,Sweden,
Britain,Estonia,Ukraine,Turkey,Austrial,Russia,Korea,Malaysia,Singapore,Thailand,Egypt,Kenya,Somali,
Congo,Zimbabwe,South Africa,etc.